Compressive strength class |
C28/35 |
---|---|
Water-cement |
0,4 |
Frost resistance |
Good |
Binder |
Portland cement |
Thickness |
0–10 mm, in holes up to 50 mm |
Grain size |
< 0,25 mm |
Air content |
4–6 % |
Water requirements |
approx 0,8 liters/4,5 kg |
Material consumption |
approx. 2,0 kg/m²/mm |
Workplace temperature |
10–25 °C |
Mixing time |
3–4 min |
Operating time 20 ° C |
45–60 min |
Begins to cure |
approx. 60 min |
Post-watering |
72 hrs |
Color |
Grey |